The CIL process is viable if there is sufficient gold content carbonates clays in the ore which will rob some gold in solution and it leaches in 8 13 hours A Stainless Steel Cathode from the electrowinning cell in the gold room Notice the gold that has plated onto the surface of the stainless steel mesh